Cost
What Sealing Actually Costs
The running cost nobody quotes you when you choose a decorative finish. Published rates, the intervals that decide the real bill, and the two calendar rules that catch people.
Choosing a stamped or coloured surface is normally treated as a one-off decision with a one-off price. It is not quite. A decorative slab carries an upkeep cost that a plain broom finish largely does not, and it comes round on a cycle that does not stop while the house is yours. Nobody hides it, exactly. It simply does not come up while a pattern is being chosen.
What the national guides publish
These are third-party figures, gathered from across the country, not prices from anybody who would come to your address. They are here to give you a scale to argue with.
| Item | Published figure |
|---|---|
| Cleaning and sealing, per square foot | $1 to $3 |
| Two-car driveway, acrylic or polyurethane | $575 to $1,700 |
| Two-car driveway, epoxy or polyaspartic | Up to $5,200 |
| Patio around ten by twenty feet | $250 to $600 |
| Labour alone | $0.70 to $1.25 a square foot |
| Sealer, by the gallon | $30 to $80, covering 200 to 500 sq ft |
| Pressure washing beforehand | $0.35 to $0.75 a square foot |
| Minimum call-out | $150 to $300 |
Two things in that table are worth pausing on before the headline rate.
The minimum charge is the first. On anything small, a path or a set of steps, the job is priced by the visit rather than by the area, and the square-foot rate stops meaning very much. Grouping small sealing work with something larger is usually the only way to make it sensible.
The second is that washing is a separate line. A surface has to be clean and dry for a sealer to bond, so a price that does not mention preparation has either buried it or is not planning to do much of it.
The interval matters more than the rate
This is the part that decides whether sealing is a minor running cost or a serious one, and it has nothing to do with the price per square foot.
| Product | Reported service life |
|---|---|
| Acrylic | One to three years |
| Epoxy or urethane | Five to fifteen years |
| Stamped surfaces, recommended cycle | Every two to three years |
Put the two tables together and the arithmetic does something unintuitive. The cheaper product applied to a driveway is not obviously the cheaper decision, because it may want doing three or four times inside the period the dearer one is still working. The expensive sealer can be the economical one, and the only way to know is to ask which product is being quoted and what its stated life is.
That question is also a decent test of whoever is quoting. A contractor who answers it immediately has chosen a product deliberately. One who does not have the answer has chosen whatever was in the van.
Two calendar rules that catch people
Both are the sort of thing you only discover at the wrong moment.
New concrete waits. Published guidance is to leave a new driveway at least thirty days before sealing it. There is one exception worth knowing about: a liquid cure-and-seal coating is designed to be applied without waiting for the slab to cure first, and it is the only category that works that way. If somebody offers to seal a slab poured last week, that is the product they should be naming.
The weather window is narrow. The recommended conditions are spring or autumn, with the temperature staying between 50 and 80 degrees for at least twenty-four hours, on a surface that is completely dry. Around here that is a real constraint rather than a formality. It removes most of the winter, a good deal of the shoulder season when the ground stays damp, and any week following heavy rain.
Which is how a two to three year cycle quietly becomes a four year one. The year gets away, the window closes, and the job moves to next spring.
What sealing does and does not do
Worth being precise, because the claims made for sealers are broader than what they do.
It keeps water, oils and grease out of the concrete. That is the whole mechanism, and it is more valuable than it sounds in this climate: water absorbed into a slab and then frozen is what drives surface damage, so keeping it out is genuine protection rather than cosmetic.
On a decorative surface it also protects the colour, which fades under sun like anything else, and it keeps the pattern reading as a pattern rather than as a grey texture.
What it does not do is fill cracks. Sealers are explicitly not a crack repair, and a slab that needs work needs that work done first and paid for separately. A quote that treats sealing as a remedy for a damaged surface has the order wrong.
What this means when you are picking a finish
Not an argument against decorative concrete. It is an argument for pricing it honestly.
A broom-finished slab can be left alone more or less indefinitely and will simply weather. A stamped one is on a cycle, and over fifteen years that cycle is a real number that belongs beside the installation price when you are comparing the two.
So ask for three things at the estimate: whether the finish you are choosing wants sealing at all, what the recommended interval is for it, and roughly what an application would cost at your square footage. Any of us should be able to answer all three standing in your garden.
How the finishes differ in the first place, before upkeep enters into it, is set out in what stamping and colour each actually add. If you have not settled on a surface yet, our concrete patio page is the place to start.
Sources
- HomeGuide, concrete sealing cost - national averages for sealing and cleaning, sealer prices by type, reported service life by product, the thirty-day rule on new concrete and the temperature window. Page dated 21 November 2025, read 22 September 2026.